Thanks Mr Mahaboob,

 

Now I can use same qualification for dissimilar material as described below.

 

Regards,

 

Surendra

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of muneebslsa@gmail.com
Sent: 12 November 2018 14:53
To: materials-welding
Subject: Re: Re: Re: Re: [MW:28618] Welder qualification

 

I have individual qualified welders per BPVC Section-IX-2015, as per following detail:

1. P1,G1 TO P1,G1

2. P8,G1 TO P8,G1

Can I use the same welder for welding of following?

1. P1,G1  TO P8,G1 

 

REPLY:

Read QW-350 will describe you the most common factors affecting the essential variables of process like dimater, thickness, t weld depostions, main factors in your case listed as per below,

1) Approved procedure (WPS) for your dissimilar.

2) Should not be change in F-no (WPS vs WPQ-Performance) same F.

3) Should not omit inert gas backing on the job.

4) Lastly clarity on P1,G1 TO P1,G1 and P8,G1 TO P8,G1 qualified welder to P1,G1  TO P8,G1 disimilar, for this scenario both welders can weld as this scenario will not have omit in backing gas , with same F nos on job and as per QW-423 table.

5) Refer QW-350, 408.8, QW-423 and QW-433

Concluding that if your production ensured with all common and main factorts above, then yes you can.

Regards,

Mohamed Muneeb Mahaboob

CSWIP 3.2-89247/2

AWS-CWI (2007)

ASNT-NDT-L2-RTFI-RT-UT-MT-PT.

SA SAP#:70021650 JAPID, QCS & QCI.

M +91-636-955-7189 & +91-801-521-6854.

From: Surendra

Date: 2018-11-12 13:22

Subject: [MW:28617] RE: 28616] Welder qualification

U r correct!

 

-----Original Message-----

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Souravbohray

Sent: 12 November 2018 11:17

To: Materials & Welding

Subject: [MW:28616] Welder qualification

 

Can't use because change in P no Nd u dnt hv qualified for p8 to p1. You have only p1 to p1 and p8 to p8.

you have qualified cs to cs and as to ss.

But u dnt hv qualified ms to ss .it's different u cnt use .if I m wrong correct me.

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.

Date: 2018-11-12 12:46

Subject: [MW:28616] Welder qualification

Can't use because change in P no Nd u dnt hv qualified for p8 to p1. You have only p1 to p1 and p8 to p8.

you have qualified cs to cs and as to ss.

But u dnt hv qualified ms to ss .it's different u cnt use .if I m wrong correct me.

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.

 

From: Ramesh

Date: 2018-11-12 12:44

Subject: Re: [MW:28615] Welder qualification

Hi

 

Pl refer QW-350 for the essential variable for Welder.

 

QW-351 GENERAL " A welder shall be requalified whenever a change is made in one or more of the essential variables listed for each welding process."

 

WPQ is not only depend on P numbers, there are other variables are also to be considered.    

Pl check your essential variable against your welding process.

 

Example For SMAW,

 

Change in base metal  P no is essential variable, i.e. QW- 403.18

 

 

Thanks and Regards

 

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"

 

 

On Sun, Nov 11, 2018 at 7:49 AM Surendra <skchordia.bhl@gmail.com> wrote:

Hello,

 

I have individual qualified welders per BPVC Section-IX-2015, as per following detail:

 

1. P1,G1 TO P1,G1

 

2. P8,G1 TO P8,G1

 

Can I use the same welder for welding of following?

 

1. P1,G1  TO P8,G1 

 

Thanking You,

 

Surendra

Bhilwara, Rajastha(Ind)

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...