Skip to main content

Re: [MW:28594] STEEL GRADES S460NL & S500ML

M---Thermomechanically treated. Generally there are 3 impact requirements in joules. J, K, L. 27joules for J. 40joules for K & 60joules for L at tested temp. For more understanding pl ref EN 10020

On Wed, 7 Nov 2018 6:03 pm Hani Al Masry <hanyonalfy@gmail.com wrote:
HOW ABOUT   S500ML 
What is M and L OR NL OR ML? 
Can you send me the copy of standards of each one?
also EN 10025-4:2004  and DIN EN 10025-3 which you refer to?

Regards,
H.A
 

On Tue, Nov 6, 2018 at 10:53 AM rajesh kaswala <rajeshkasvala@gmail.com> wrote:
  S460NL acc. to DIN EN 10025-3 Mat.no. 1.8903 S460NL is a weldable, normalised steel for steel constructions, with high yield strength combined with high toughness to save weight in use.
 Delivery with certificate 3.1 to DIN EN 10204. 
Chemical composition (heat analysis %) Grade C max. Si max. Mn P max. S max. Al min. Cr max. Mo max. Cu max. Ni max. V max. N max. Nb Ti S460NL 0,20 0,60 1,00- 1,70 0,025 0,020 0,020 0,30 0,10 0,55 0,80 0,20 0,025 0,05 % 0,05% 
Mechanical properties in delivery condition Tensile testing on transverse specimens at room temperature Grade R m (MPa) ReH (MPa) A5 (% min.) 
Thickness mm  100 > 100  200  16 > 16  40  40  63 > 63  80 > 80  100 > 100  150 S460NL 550 - 720 530 - 700 460 440 430 410 400 380 17 
impact values (KV) carbon equivalent values (CEV) transverse 27 Joule -50°C  63 mm 0,53 longitudinal 16 Joule -50°C  63  100 mm 0,54 

  regard
rajesh

On Sun, Nov 4, 2018 at 8:29 PM Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear Exerts 

what is Steel Grades S460NL & S500ML Are this is CS or it is alloy steels like HARDOX , WELDOX and now they call it Domex?

what is it is specification ? standards? recommended usage and applications?

Regards,
H.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...