Re: Re: [MW:28592] Golden Joint Repair Penalty

Explain your client that penalty comes under % coverage where there is a failure, when a weld is considered as mandatory RT 100 % it is like an additional joint and 100% services do not required any penalty regardless of lineclass.

If really you wanted to cover your lineclass then you wouldnt be giving golden joint as 100%.

It is to be understood.

Regards,
M.Muneeb.



 
Date: 2018-08-12 18:49
Subject: Re: [MW:28196] Golden Joint Repair Penalty
In this case an additional NDT, say UT is advisable. Please discus with your client.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Monday, 6 August, 2018, 9:19:22 AM IST, Bishwambhar Kumar <bishwambhar10@gmail.com> wrote:


Dear Experts,
                     We have repair in Golden joint and it is successfully done. But now client is asking for penalty for this joint as it was a 5% RT line.
But as per my understanding as it is a Golden Joint ( a 100% RT joint), so no need of repair penalty. But I am not getting any code reference to it. Please help me to find any reference.

Thanks and Regards,

Bishwambhar Kumar
Ph:- +974-55311582


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .