Re: Re: [MW:28605] Combined PQR

Let us not confuse ourself. It is clearly mentioned that we can combine  different WPS within the limitation.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Nov 9, 2018 at 8:03 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
Hi just to be sure we are not diverting away from the topic.

The question was "whether separate WPS's can be written from a multi process PQR."

ASME is very clear when it comes to deriving processes separately in a WPS from a multi process PQR.

However if you refer AWS D1.1, nothing is stated with respect to the same. When it is not stated, then it cannot be followed. 



On Thu, Nov 8, 2018 at 10:41 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:

Hi

 

If you see both ASME (QW-200.4) & AWS (Clause 3.6.1) on combination of weld procedures , both code does not talk about PQRs. Only the final WPS ( Each WPS may include

one or a combination of processes, filler metals, or other variables. )




 

Ƙ  AWS provide is simple explanation in this regard than ASME

Ƙ  Both codes does not talk about separation of PQRs ( combination is important than separation)

Combination of WPS/ PQRs may NOT be already welded earlier, but separation is done for the already welded process, it is not important criteria, I believe)

 

 (Under ) QW-200.2 – ASME

 

 

(Under pre-qualified) C-3.7 General WPS Requirements - AWS


 

In summary, Both codes  have intention to combine  WPS/PQR provided all the essential variables for each process is meeting the limitations specified which results successful production welds either with combination or Separation. 

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Tue, Nov 6, 2018 at 12:23 PM muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:
When it said ''A combination of qualified and prequalified WPSs may be used without qualification of combination''   it means it is very clear that the combination of multiple qualified or pre qualified WPSs can be used if the limitation of essential variables applicable to each process is observed. 

So PQR has nothing to do here.

But whether AWS D1.1 allows Multiple WPSs With One PQR/Multiple PQRs With One WPS? 

Regards,
Muneeb.M




 
From: Ramesh
Date: 2018-11-02 09:12
Subject: Re: [MW:28554] Combined PQR
Hi Nithin,

i am unable to find the word " independent PQR's may be combined " in above clause

i presume, this clause does not say about PQRs, Only your final WPS ( which may have single supporting PQRs or process or combined PQRs or process) 

These qualified WPSs can be combined  without combination and within limitations of each process ( refer last two para carefully ) 

i understand from response that, suppose if an PQR have with combination process ( Ex.TIG+SMAW)  , u are interpreting that preparing Two separate WPS ( one for TIG & one for SMAW)  is not allowed as per D1.1. right ? 

or, Pl explain your interpretation of above 3.6.1 clause.  


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Fri, Nov 2, 2018 at 10:30 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
Dear Mr. Rameshkanna,

Note that clause 3.6.1 clearly states independent PQR's may be combined and does not state WPS's can be made from the combination PQR.

On Thu, Nov 1, 2018 at 7:54 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:

Hi 

shakin thobias

 

1. Please refer AWS D1.1 , Part C for performance qualification requirements.

Range of qualifications - pl refer Table 4.10 & 4.11

 

2. Combination of WPS is allowed as per 3.6.1  This is applicable for both qualified or prequalified WPS.[ Screen shot from 2015 edition as below ]


image.png

Also refer OLD AWS interpretation as below [ 1984 edition]

image.png




Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Oct 31, 2018 at 10:06 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
In AWS there is no provision of extracting a process. for eg, you are qualifying FCAW+SMAW, you have to use same combination on job too. Writing separate WPS for SMAW & FCAW is not acceptable as per AWSD1.1.

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...