Re: [MW:28348] testing of inaccessible welded joints

It is not possible since all of joints butied.
Does anybody know about high resolution MFL would be useful in evaluting of joint
Regards.

On Thu, Sep 27, 2018, 11:15 AM 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Try Crawler RT

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Thursday, 27 September, 2018, 12:30:25 PM IST, Ali Asghari <asgharialigl@gmail.com> wrote:


Do you have any file for presenting this method?
I said in previous emails, pressure testing may not detect some rejected defects that don,t cause leak.
Regards.

On Thu, Sep 27, 2018, 5:45 AM pradip kumar Sil <pradipsil@gmail.com> wrote:
Borodcope you can identify internal defect. otherwise pressure test


On Mon, 24 Sep 2018, 13:01 Ali Asghari, <asgharialigl@gmail.com> wrote:
Thank you for responding but our line is long& we want to know about internal defects and visual in that situation doesn't have good sensitivity.
Actually, I am wondering about mechanised ultrasonic that syncronised with crawler.
If you know any equipment or company that have simillar technology.
Regards.

On Mon, Sep 24, 2018, 8:37 AM sandeep kumar <sandeepdhiman63@gmail.com> wrote:
for smaller length, a surface inspection with boroscope can be possibly made. Now a days boroscope with robot manipulator (pipe crawler) also available which can be remotely controlled although a costly matter.

The above system can be used upto 500 mm however diameter restriction is applicable.


Shared more details about the joint types, pipe dia length etc would be better for the understanding.

Thanks & regards
Sandeep Kumar

On Sunday, September 23, 2018 at 3:17:28 PM UTC+3, Ali Asghari wrote:
Dear Kumar.
this line is piggable but I don't think the pig with considering pf it's velocity don't have ability to scan welds?if you know information or experience, please let me know.
pressure testing can only detect defects that cause leak or rupture, and other rejected defects can be undetected.

Regards.

On Sun, Sep 23, 2018 at 1:32 PM Lakshmankumar Bayyana <lakshma...@gmail.com> wrote:
If it is a pipe line, best option is to do hydro test with 1.25 times of the working pressure to ensure the integrity 
Also can go with ultrasonic pig in case of pig possible lines

Thanks and Regards 
Lakshman kumar. B 
+91 9440031459

Sent from my iPhone

On 23-Sep-2018, at 11:28 AM, Ali Asghari <asghar...@gmail.com> wrote:

Dear All.

Does anybody know there is NDT method that can inspected welded joints which are buried and not accessible?our concern is about finding of construction defects either surface and internal that have a good detect ability for linear ones particularly Transverse Crack.

Regards.
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U-K3LErE3mU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U-K3LErE3mU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U-K3LErE3mU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U-K3LErE3mU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...