Skip to main content

Re: [MW:28309] Conflict between ASME Section IX clause QW 404.12 & WQ 404.33

allow me to add that 404.12 is applicable only when impact testing is required by the design & construction code. It appears under the column "supplementary essential variables".
404.33 in all processes, except for resistance welding, appears under the column "non essential variables". For resistance welding is essential

Στις Τρί, 18 Σεπ 2018 στις 7:39 π.μ., ο/η sandeep kumar <sandeepdhiman63@gmail.com> έγραψε:
Thanks Vivek. Its clear my some doubts

On Monday, September 17, 2018 at 3:23:29 PM UTC+3, Patel Vivek wrote:
Hi Sandeep,

404.12 -


1) if impact is applicable ER70SG or ER90SG is a special designation. All " G" is a special filler or electrode we can't use different in WPS. we have to use the same we used during PQR.
 
2) and following things do not require requalification. you can change in the WPS regardless with what you qualified the PQR.

                



While 404.33 -

1) you can switch within SFA classification or use different manufacturer.


2) when organization mentioned something on WPS like E7018-H4R then organization have to use the same. you can not weld with E7018-1. when you mentioned something on WPS means follow the same.


I hope this clears your apprehension on QW-404.12 & QW-404.33.


Regards,
Vivek Patel


On Mon, Sep 17, 2018 at 1:28 PM, sandeep kumar <sandeep...@gmail.com> wrote:
Dear all

Kindly give your views on the interpretation of ASME Section IX clause QW 404.12 & WQ 404.33 when SMAW & GMAW process are concerned.
My point, as both the variables are same for Change in Filler metal classification, QW 404.12 is a supplementary variable while the QW 404.33 is non-essential variables.

There are additional information in QW 404.12 compare to QW 404.33 however focused point i.e. ''A change in the filler metal classification within an SFA specification'' is same.

Thanks a lot.

Regards
Sandeep Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Warm Regards,
Vivek patel
+91-9824874732

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...