Monday, July 2, 2018

[MW:28015] consumable selection

Good Morning friends,

I would like to know how we chose the consumable.
suppose I need to qualify a WPS P1Gr1 to P1Gr1.

how I chose the consumable from scratch? could anyone please mention where its in the spec.
also how I chose the gas or combination of gas ?

thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone