Crude oil storage, does it have to comply with NACE MR0175/ISO 15156?


QUESTION:
Crude oil storage and handling facilities operating at a total absolute pressure below 0.45 MPa. My understanding of the above paragraph is that, it includes only dead oils with no gas in equilibrium. If any gas is in equilibrium with a crude (operating less than 0.45 MPa) which contains H2S more than 0.3kPa (in the gas phase), the whole system is considered as sour. I need your advice for my understanding, if correct or not?


ANSWER:
Crude oil storage and handling facilities means that it is dead oil and H2S/CO2 have been removed. The very low residual amount is considered negligible. This is the reason why these facilities are permitted exclusions from the standard. However, it is up to the user to check that these statements are true for the considered facilities.

Ref# MP INQUIRY #2009-14

https://www.linkedin.com/groups/122787/122787-6419419780360609792

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...