Re: [MW:24136] what is the difference between QAP and ITP


Dear Sirs


   QAP :- Usually describes  how will you manage the Quality System

Eg:

1.       Project Management strategy

2.       Applicable documents

3.       Management system & Responsibility

4.       Project execution

5.       QA/QC

6.       Marketing, design, Procurement ,Production, store

7.       Resource management

8.        Product realization

9.       Measurement analysis &improvement

10.   HR & logistics

11.   Project Organogram

 

ITP:-solely related  to QA/QC this will describe all the various stages of inspection and testing from start to finish requirements of a product.

     Generally this will include monitoring, Review, witness and hold points   listed for all relevant parties and this is approved prior to commencement


Regards

M.S Nair.G


On Tue, Jan 19, 2016 at 10:53 AM, Lakshman <lakshmankumar4@gmail.com> wrote:

Hi,

 

ITP – Inspection test plan includes tests, its acceptance tolerance, type of instruments used, its accuracy etc –

Ex –

Pipe thickness – ultrasonic method, XXX instrument, nominal thickness 10mm, acceptable "-0mm +1.6mm" etc, frequency each pipe measured from outside, at 6 locations, procedure for testing – as per Doc # - XXXXX

ITP is a in house document of a manufacturer. (in some complicated cases, and close tolerance requirement cases clients asks for ITP also)

In ITP manufacturing process also defines, but where as in QAP it is not required.

 

Whereas QAP means it's a quality plan and broad details will be their…

Ex- Pipe,

Thickness, Dia, Length

Frequency – each pipe

Acceptance norms – Client spec / ASTM code / Project spec / approved drawing etc

Client witness / TPI witness etc

QAp is a client approval document.

 

 

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kadir godil
Sent: Tuesday, January 19, 2016 8:45 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:24128] what is the difference between QAP and ITP

 

ITP is given by customer which covers only main inspection calls e.g. full component after welding UT of only some joints, final machining dimensions and after assembly inpection whereas QAP is made by the manufacturer which covers all the stage wise inspection..

 

On Tue, Jan 12, 2016 at 4:14 PM, Pradip Ghosh <pradipg2@gmail.com> wrote:

 

Can any one provide me a details explanation of difference between QAP and ITP.

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5107353-54a0-49a9-9d23-6123ee54d599%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BVeSfvN1fLsv_-qmu0uPZk4C_HpwW305agu3y9TgPM-YA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/002801d15279%247cc6f870%247654e950%24%40com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq7HUCj5CAASB%2B5OW_P71npZ%2B1wU%3DJk7-O1ShgLvj%3DpnNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...