Skip to main content

Re: [MW:24072] Re: Type of paint use on fit up joints before welding

Dear .

I would like to inform you selection of paint are based on type of environment use like corrosive & its applicability use.

There is wide range of paints are available with minimum expected life.

Regards
Dinesh

On Friday, January 8, 2016, Ki Rok, NAM <kirok.nam@gmail.com> wrote:
Apology for late reply.

Hope that below comments can support for solution of curiosity

Our Company has been coated with an aluminum-flake weldable primer ("Deoxaluminite" or "Bloxide" or other brand) for prevent the anti rust of Weld Bevel Ends.

2010년 11월 11일 목요일 오후 3시 24분 23초 UTC+9, Shamesh Lotlikar 님의 말:


Dear All,

can any one give information on type of PAINT which we can use on the fit up joints before welding so that it will prevent the rusting of the surface of fit up joints. Kindly give us the name and type and brand of the paint which will be faster to get the same

Shamesh Lotlikar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/15d4ea6f-4b48-4ab9-9c86-4811d748bd57%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135

असो द्यावी दया तुमच्या लागतसे पाया.

Pray for others, sometime, You might never need to pray for yourself again.....

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrUbMzfy2H3avf21hSSYOMX%2Baj91z0iEgtM2_JHFcmG0Hg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...