RE: [MW:24123] Fwd: mode of metal transfer

ASME II Part C SFA-5.20/SFA-5.20M

 

A7.1 EXXT-1C and EXXT-1M Classifications.

Both the EXXT-1C and EXXT-1M electrodes have similar type slags and are designed for single and multiple pass welding

using DCEP. The larger diameters (usually 5⁄64 in. [2.0 mm] and larger) are typically used for welding in the flat position and for welding fillet welds in the horizontal position. The

smaller diameters (usually 1⁄16 in. [1.6 mm] and smaller) are typically used for welding in all positions. These electrodes are characterized by a spray transfer, low spatter

loss, flat to slightly convex bead contour, and a moderate volume of slag, which completely covers the weld bead.

Electrodes of this classification have a rutile base slag and have the ability to produce high deposition rates.

With Regards

 

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de udaya bhaskar
Enviado el: domingo, 17 de enero de 2016 06:39 a.m.
Para: materials-welding@googlegroups.com
Asunto: [MW:24119] Fwd: mode of metal transfer

 

 

Dear experts,

 

Please clarify which mode of metal transfer we are used  in FCAW 

 

 Welding Process : FCAW

Gas                      : co2

Filler wire             : AWS A5.20 71T-1C

Mode of metal transfer : ? (Please clarify )

 

 

--

With Regards

 

Udyabahaskar.D

 

+919676270121

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RN2REbTDX4rvKdo1oUtWMZMz09KaPEPi9TLi70tg5M-BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



__________ Información de ESET Endpoint Security, versión de la base de datos de firmas de virus 12885 (20160118) __________

El mensaje fue verificado por ESET Endpoint Security.

http://www.eset-la.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...