Tuesday, May 5, 2015

Re: [MW:23209] RE: 23206] Failed SSC test

Hi Alan
Based on the same WPQT but conducted on different test coupon the highest hardness value is 244 on the HAZ side.
Do you reckon hardness is the issue?

Thanks.
Amir Zakee

Sent from my BlueBerry 10 semakphone.
From: Alan Denney
Sent: Selasa, 5 Mei 2015 20:23
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:23207] RE: 23206] Failed SSC test

Boxbe This message is eligible for Automatic Cleanup! (alan@denney1.freeserve.co.uk) Add cleanup rule | More info

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone