Tuesday, May 5, 2015

[MW:23207] RE: 23206] Failed SSC test

Have you checked the hardness of  the heat affected zone on the carbon steel side? Do you have the results and a macro?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Amir Zakee Adnal
Sent: 05 May 2015 12:29
To: materials-welding@googlegroups.com
Subject: [MW:23206] Failed SSC test

 

Dear experts

I conducted a transition joint of API 5L X65QO (carbon steel) + API 5L X65QO internal clad with 3mm Alloy 825.(CRA)

I passed all the mechanical testing but failed the SSC test as the specimens crack along the fusion line on the carbon steel side. I used GTAW/SMAW with special metal 625 for GTAW and Special metal 112 for SMAW.

For the carbon steel to carbon steel test coupon i passed the same SSC test while the CRA to CRA I only need to do G48 test which I passed.

Can somebody point out the probable root cause of the crack and what is the way forward if I need to pass this test.

 

Thank you.

Amir Zakee

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGtokWad0PyJk7%3Dyp%2Bxr%3DQK1cKz-LMMyWDJOGvWdZ9hr1MOLxw%40mail.gmail.com.