Re: [MW:21785] Change in soaking time

Yes if all other parameters are same
 
With Best Regards,
Shashank C Vagal


On Tuesday, 2 September 2014 9:17 AM, pradip kumar Sil <pradipsil@gmail.com> wrote:


Daear All,
I have one wps for ASTM A335 GR P11 material with one hour soaking time.  Can i use this wps for same material with 2 hour soaking time. 
Ragards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone