Skip to main content

Re: [MW:21696] Welder Qualification

Tack.1 ..Removal type no need because that potrion welded by unqualified welder does not going to be included in final weld.

Tack 2.Non removable type  Qualified welder required as per code.

So it is important you note what type of tacking is ongoing. Like...Bridge tack or something else. Again manufacturer can say they going to remove these unqualified welder welded tacks during the welding.

Regards
Shridev

On 25 Aug 2014 17:12, "Dhanabal Jalachandran" <dhanabal.jalachandrann@gmail.com> wrote:
Dear,

Regarding point 2, as you have said, 

The tack welding is going to be removed.? so the welder may or may not be qualified.? Kindly suggest.

Point 2-As per code you need to qualified welder for tack weld also because it depends whether tack become part of welding aur you are going to remove it also material, service conditions of equipment.

BR
Dhanabal Jalachandran


On Mon, Aug 25, 2014 at 12:14 PM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear,

Point 1 If a welder is qualified in CS for GTAW process then he is qualified for SS with gas backing Argon because for GTAW process deletion of gas backing is essential variable if you carefully go through CODE and for GTAW filler wire SS and CS
both falls in F NO 6 AS given in code. So CS qualified welder cam make weld in SS and for P no welder is qualified to weld in P1-P15, P34, P41-P43 etc. As per code.

Point 2-As per code you need to qualified welder for tack weld also because it depends whether tack become part of welding aur you are going to remove it also material, service conditions of equipment.

Point the 3-If both codes requiement filled and after client approval welder is qualified.
Best Regards,
Mohit Aggarwal.

On 25-Aug-2014 2:10 PM, "Dhanabal Jalachandran" <dhanabal.jalachandrann@gmail.com> wrote:
Gent's,

Kindly need your advice to clear one issue based on Welder Qualification.? These questions were asked to me yesterday in Aramco Interview.

  • If a welder is qualified with CS, can he weld SS.? ( i answered he cannot as F4 and F5 doesn't allow as per ASME Sec IX), but the interviewer told me it can be welded in GTAW with some kind of Gas i forgot the name of it. but i have gone through all the reference code i dont find any as P number and F number are essential variable.

  • Welder requires tack welding qualification in ASME Sec IX or AWS D 1.1.? As per ASME Sec IX all the welders need to be qualified. As our company manufactures only Tanks and Vessels not much involved with AWS D 1.1, is there any applicable stuff where specifically welder needs to be qualified for Tank welding if he is not qualified welder.??

  • If a welder is qualified with ASME Sec IX, can he weld the jobs with the code based on AWS D 1.1.? I have answered yes it's possible as the requirements need to be followed, i.e., Essential variable, Client approval as per AWS D 1.1 Clause 4.2.2.1
 
Regards
Dhanabal Jalachandran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards
Dhanabal Jalachandran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...