Re: [MW:21692] Welder Qualification

Dear,

Point 1 If a welder is qualified in CS for GTAW process then he is qualified for SS with gas backing Argon because for GTAW process deletion of gas backing is essential variable if you carefully go through CODE and for GTAW filler wire SS and CS
both falls in F NO 6 AS given in code. So CS qualified welder cam make weld in SS and for P no welder is qualified to weld in P1-P15, P34, P41-P43 etc. As per code.

Point 2-As per code you need to qualified welder for tack weld also because it depends whether tack become part of welding aur you are going to remove it also material, service conditions of equipment.

Point the 3-If both codes requiement filled and after client approval welder is qualified.
Best Regards,
Mohit Aggarwal.

On 25-Aug-2014 2:10 PM, "Dhanabal Jalachandran" <dhanabal.jalachandrann@gmail.com> wrote:
Gent's,

Kindly need your advice to clear one issue based on Welder Qualification.? These questions were asked to me yesterday in Aramco Interview.

  • If a welder is qualified with CS, can he weld SS.? ( i answered he cannot as F4 and F5 doesn't allow as per ASME Sec IX), but the interviewer told me it can be welded in GTAW with some kind of Gas i forgot the name of it. but i have gone through all the reference code i dont find any as P number and F number are essential variable.

  • Welder requires tack welding qualification in ASME Sec IX or AWS D 1.1.? As per ASME Sec IX all the welders need to be qualified. As our company manufactures only Tanks and Vessels not much involved with AWS D 1.1, is there any applicable stuff where specifically welder needs to be qualified for Tank welding if he is not qualified welder.??

  • If a welder is qualified with ASME Sec IX, can he weld the jobs with the code based on AWS D 1.1.? I have answered yes it's possible as the requirements need to be followed, i.e., Essential variable, Client approval as per AWS D 1.1 Clause 4.2.2.1
 
Regards
Dhanabal Jalachandran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .