Dear Sirs,

 

I have a different opinion :

 

When reading EN10204 in detail , I understand that this document is to describe how to classify type of CMTR ( mill certificate ) and specify criteria / condition of each type.

 There is no clause be stated that CMTR shall have the wording “ according to EN10204 type xxxx “ be shown in CMTR.   So if a specific CMTR is showing the required contains which fully comply with the requirements of EN10204 ( such as properties per standard’s requirement and signature of QA/QC manager which is not under production , etc. ) , such CMTR should be able to be classified as a certain type of CMTR per EN10204 for example type 3.1 or type 2.2.

 

This can be a problem many times when the work must be executed under the contract which state that CMTR of steel shall be type 3.1 per EN10204 and then fabricators face a lot of difficulties to find material available in the stock of the market or even from the local steel mill to get CMTR which show wording “ According to EN10204 type 3.1 “ even though all of test result and chemical compositions and signature of authorized person are fully conform to requirement of type 3.1 criteria per EN10204.    The point is in some markets / countries or some makers do not care or not willing to put such wording on their CMTR and cause difficulties to a fabricator to get the required material in such constrain. 

 

I believe that under such situation , there should be some relaxation and CMTR should be allowed to be used on case by case basis after verify contains in CMTR.

 

Regards,

C.Nopadon

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vairamuthu Ramar
Sent: Thursday, June 26, 2014 9:56 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:21265] EN 10204 type 3.1 requirement

 

Definitely Yes.
 

 


Date: Thu, 26 Jun 2014 11:33:25 +0530
Subject: [MW:21260] EN 10204 type 3.1 requirement
From: sadiq.mech@gmail.com
To: materials-welding@googlegroups.com

Dear Members,

 

Is it mandatory to be written as EN10204 type 3.1 on MTC if it is required by client?

 

Thanks & Regards,

 

Mohd. Sadique Sheikh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...