ABSOLUTELY!!
316L BASE METAL, THE FILLER METALS COULD BE 316L (SMAW) 316L/316LSI (GMAW) 316L(GTAW) 316L(SAW).
IF YOU CHOOSE MIG WIRE, YOU SHOULD USE 316LSI. BECAUSE "SI" CAN OPTIMIZE THE WELDING POOL, AND MAKE THE BEAD LOOK GOOD.
IN ONE WORD, 316LSI IS GOOD FOR WELDING BEAD.
ROY
BWG
Dear Experts,
the subject filler ER316Lsi was rejected by the client at Kazakhstan can you explain the silicon factor and can i use it on 316L stainless steel lines that we use for sewage water treatment ? please advise.
Best Regards,
Eng. / Mohamed El Sayed
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment