Remember that E-7018 is F4 and  6013 is F3, In procedure is essencial variable.But in performance welder there is not problem

 

 

 

Regards

Carlos Oliveros

Mechanical  Inspector/ Eng.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...