Wednesday, August 1, 2012

Re: [MW:15006] change in electrode class

Dear Sir,
 
 As per ASME 2011 Addenda Edt., IS 2062 Material as add so its comes under P No 1 & G no 1. WPS & PQR can be used with the same G.No & P No, for your references find the attached page.
 
Thanks & Regards,                                                    
Karthick.D
Ph.No: +971-507655957 (UAE)

On Wed, Aug 1, 2012 at 9:04 AM, <pankaj.kolhe@wipro.com> wrote:

Dear all,

If the procedure is qualified on E7018 Electrode for SA 516 Gr 70 then can we use this WPS/PQR for welding IS2062 Gr B by E6013 electrode. Also for welder qualification can we use this WPS/PQR , Give code reference

I think change in filler metal class is essential variable.

 

With Regards,

Pankaj Kolhe

QC

Wipro Water (Wipro Ltd)

O- + 91 22 39302135

M: +91 9323940892

 

Wipro Limited.Serene Properties Private Limited,Special Economic Zone,3rd Floor,Building No. 7, Plot No.3,TTC Industrial Area,Thane Belapur Road,Opposite Airoli Rilway station.Airoli, Navi Mumbai- 400708,Maharashtra

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...