Thursday, August 2, 2012

[MW:15008] RE: change in electrode class

Dearr sir,

But my question is

I have a qualified WPS/PQR for P1 G1 with E7018 Electrode and another welder is qualified with same electrode.

Now can another welder qualified with E7018 can weld IS 2062 with E6013 electrode?

Can I offer this WPS/PQR of E7018 to TPI for this E6013 welding.

Pankaj

 


From: John Henning [mailto:jhenning@deltak.com]
Sent: Thursday, August 02, 2012 2:42 AM
To: Pankaj Kolhe (WF01 - WIN Water)
Subject: RE: change in electrode class

 

WPS may not be used as indicated.

Per QW-253, F-no is an essential variable for SMAW procedure qualification, i.e. QW-404.4 applies.  E7018 is F4 while E6013 is an F2.  Therefore a PQR using an F4 electrode cannot support a WPS using an F2 electrode or vice versa.

As long as impacts are not required, base metal would not be an issue since 2011a Section IX QW/QB-422 recognizes  SA/IS 2062 E250 B as a P-No. 1, G-No. 1 material.  If impact testing was required the

With respect to weldor performance qualification. {Assuming you had a properly qualified WPS for F2, F3, or F4 electrodes.}  The weldor could use either F2, F3, or F4 electrodes and be qualified for welding with F2 electrodes per QW-433.

John A. Henning

Welding & Materials

 

From: pankaj.kolhe@wipro.com [mailto:pankaj.kolhe@wipro.com]
Sent: Wednesday, August 01, 2012 12:05 AM
To: materials-welding@googlegroups.com; John Henning; pgoswami@quickclic.net
Subject: change in electrode class

 

Dear all,

If the procedure is qualified on E7018 Electrode for SA 516 Gr 70 then can we use this WPS/PQR for welding IS2062 Gr B by E6013 electrode. Also for welder qualification can we use this WPS/PQR , Give code reference

I think change in filler metal class is essential variable.

 

With Regards,

Pankaj Kolhe

QC

Wipro Water (Wipro Ltd)

O- + 91 22 39302135

M: +91 9323940892

 

Wipro Limited.Serene Properties Private Limited,Special Economic Zone,3rd Floor,Building No. 7, Plot No.3,TTC Industrial Area,Thane Belapur Road,Opposite Airoli Rilway station.Airoli, Navi Mumbai- 400708,Maharashtra

 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India