Dear Mr. Pankaj Kolhe,
If you are using ASME SEC IX 2010 then you can not use.
For SMAW Process F number is Essential Variable for welding procedure
qualification and F Number of E6013 is 2 and F number of E7018 is 4.
And for welder qualification F number also essential variable. So you
can not use different F number.
Reference QW 432, WQ 253, QW 353
On 8/1/12, pankaj.kolhe@wipro.com <pankaj.kolhe@wipro.com> wrote:
>
> Dear all,
> If the procedure is qualified on E7018 Electrode for SA 516 Gr 70 then can
> we use this WPS/PQR for welding IS2062 Gr B by E6013 electrode. Also for
> welder qualification can we use this WPS/PQR , Give code reference
> I think change in filler metal class is essential variable.
>
> With Regards,
> Pankaj Kolhe
> QC
> Wipro Water (Wipro Ltd)
> O- + 91 22 39302135
> M: +91 9323940892
>
> Wipro Limited.Serene Properties Private Limited,Special Economic Zone,3rd
> Floor,Building No. 7, Plot No.3,TTC Industrial Area,Thane Belapur
> Road,Opposite Airoli Rilway station.Airoli, Navi Mumbai-
> 400708,Maharashtra[cid:image002.gif@01CD6FD1.6B5D7F70]
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India
Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment