Re: [MW:15004] change in electrode class

Pankaj Kolhe,

If you followed the ASME code,the IS2062 need to be requalified in spite that IS 2062 is nearer to ASTM A 36 . In another word, material IS 2062 can not be categorized into the same P No. as SA 516 Gr 70.
However,the E7018 has the same F No. as the E6018,,i.e. E6018 can be used without requalification.

hope this helps.

Regards,
Devin.

2012/8/1 <pankaj.kolhe@wipro.com>

Dear all,

If the procedure is qualified on E7018 Electrode for SA 516 Gr 70 then can we use this WPS/PQR for welding IS2062 Gr B by E6013 electrode. Also for welder qualification can we use this WPS/PQR , Give code reference

I think change in filler metal class is essential variable.

 

With Regards,

Pankaj Kolhe

QC

Wipro Water (Wipro Ltd)

O- + 91 22 39302135

M: +91 9323940892

 

Wipro Limited.Serene Properties Private Limited,Special Economic Zone,3rd Floor,Building No. 7, Plot No.3,TTC Industrial Area,Thane Belapur Road,Opposite Airoli Rilway station.Airoli, Navi Mumbai- 400708,Maharashtra

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
修延飞
Yanfei Xiu
技术中心 焊接室
Tech Center,welding department
山东核电设备制造有限公司
SNPEMC  
地址:中国山东海阳临港产业区
Address:Lingang Industrial Area,Haiyang City,Shandong Province ,PRC
TEL:15967615395


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...