Sunday, August 5, 2012

[MW:15024] Oil pipes expansion joints

Dear Experts...
 
I need your help in understanding the criteria of installing the (expansion joints) in oil pipes. I need to know the recommended distance between each expansion joint, and the recommended  material of these joints.
 
Many thanks...
 
Dr. Eng. Alaa Abdulhasan Atiyah
Iraq-Basrah 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...