Skip to main content

Re: [MW:10022] Re: LAS Grade 11 welding

Dear Sir,

Except the carbon content chemical composition are same for ER70S-B2L
and ER80S-B2 both are inentical.
Please check Annex A 7.5 of SFA-5.28 of ASME Sec IIC.

Regards

Atul Chaturvedi

On 2/26/11, JASPAL SINGH <jaspaldhesi@gmail.com> wrote:
> Dear Sir,
>
> We done some testing with ER80S-B2L in which carbon content is in
> 0.05%. There is some reservation by the consumable manufacturer if we
> ask for longer simulation, otherwise there is normal results which
> even meet the API-934C requirements also for impact. Even PTC testing
> after minimum and maximum simulation it was perfectly fine.
>
> Regards
>
> JASPAL SINGH CWI-AWS, CSWIP-3.1
> Head Quality Assurance-ISGEC-PED, Yamunanagar, Haryana (India) PH:
> +911732307251; Mob. +918930111441(CUG), +919996624244
>
>
> On Feb 25, 1:58 pm, Jignesh Desai <jignesh.desai....@gmail.com> wrote:
>> *Back Ground: *Design Code: B 31.3 / Design Temp: 415° C Max.
>>
>> Can any one send some technical data if we find less carbon then the
>> specified range (0.07 ~ 0.12) for ER80S-B2 (SFA 5.28-ASME Sec IIC)?  This
>> is
>> for welding LAS Grade 11.
>>
>> Regds/Jignesh
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .