Skip to main content

Re: [MW:10029] Tank Peaking/Banding Issue, API 650

Respected Wahab,
 
When you are applying for whole tank height then the criteria will be API 650 i.e., 1/200. Where as if you are going to check plumbness for individual shells the ASTM applicable relevent specification has to be refered. Your interpretation is correct and the tolerence for each individual shell plate based on thickness, height and length will be as per your derived value.
 
Ishfaq
Jubail, KSA

From: Abdul Wahab <awengineer@gmail.com>
Subject: Re: [MW:10024] Tank Peaking/Banding Issue, API 650
To: materials-welding@googlegroups.com
Date: Saturday, February 26, 2011, 6:12 PM

Dear Sir,
 
Thank you very much for replying, but problem is that API 650 by itself refering to mentioned standard like ASTM A 6M etc.
 
Please advice,
 
Abdul Wahab

On Sat, Feb 26, 2011 at 3:24 PM, Suresh <bobsuresh24@gmail.com> wrote:
Hii Abdul ,

You should follow API 650 for tank consrtuction , not ASME code .

In my best of my knowledge , you need to refer to API 650 and follow
tolarances which was mentioned in API 650 .

Thank you

Suresh

On 2/26/11, Abdul Wahab <awengineer@gmail.com> wrote:
> Dear All,
>
> I am Abdul Wahab working in KSA as QA/QC Inspector, I have an issue
> which is confusioning me. Below there is copy of Paragraph of API 650.
> Plumbness, peaking, banding & flat spot discussed in this & tolerances
> are provided but along with tolerance of API 650, also refering to
> ASTM standards, those standards have tolerances aproximately a double
> values as compared to API 650 Tolerances. Do we need to follow those
> as ASTM is not a tank construction code but provide guidance about
> matrial manufacturing,testing & handling etc.
>
> We have Banding Value for 6 mm Plate of 13 mm max,  can we consider a
> dent as a banding problem in tank shell.
>
> Please see below & advice.
>
> 7.5.2 Plumbness
>
> a. The maximum out-of-plumbness of the top of the shell relative to
> the bottom of the shell shall not exceed 1/200 of the total
> tank height. The out-of-plumbness in one shell course shall not exceed
> the permissible variations for flatness and waviness as
> specified in ASTM A 6M/A 6, ASTM A 20M/A 20, or ASTM A 480M/A 480,
> whichever is applicable.
>
>
>
> 7.5.4 Local Deviations
>
> c. Flat spots measured in the vertical plane shall not exceed the
> appropriate plate flatness and waviness requirements given in
> 7.5.2.
>
> If there is any confusion to understand, please ask.
>
>
> Abdul Wahab
> Mechanical Inspector
> KSA
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...