Wednesday, September 15, 2010

Re: [MW:7019] SDSS consumable procurement

Hi Limesh,
Please find below my Suggestions as marked in red.
 
Welding
 
1.PWHT - ? - N/A
 
2.Radiography/soundness test - ? N/A
 
3.Fillet weld test - ? - AS PER SFA5.4 - TABLE-3 REQUIREMENT 
4.Bend test - ? - N/A
 
5.Other .......... ? - AS PER CLIENT'S REQUIRMETS YOU CAN REQUEST-If you go for Schedule "K"
 
Chemical Analysis
 
1.Ferrite content - Found from client spec
 
2.Moisture content - ? -SHALL BE SPECIFIED IN CERTIFICATE - OPTIONAL
 
3.Diffusible hydrogen - ?-SHALL BE SPECIFED IN CERTIFICATE - OPTIONAL
 
Mechanical Testing
 
1.Yield strength - Found from ASTM - AS PER SFA5.4
 
2.Tensile strength - Found from ASTM - AS PER SFA5.4
 
3.Impact test - Found from client spec the required impact energy
 
4. Lateral expansion - ? - AS PER SFA5.4
 
4. Hardness - Found from client spec 
  
What is Test schedule according to 5.01, ie Schedule F, G,H,I,J and Schedule K?
IF THERE IS NO CUSTOMER REQUIRMRNTS/SPEC, YOU CAN GO FOR SCHEDULE - F. BUT IN YOUR CASE SEEMS TO CUSTOMER REQUIRMENT ALSO.SO YOU CAN GO FOR "K".. AND SPECIFIY THE .ADDITIONAL TEST REQUIRED BY THE CLIENT/SFA5.01.
OR OTHERWISE GO WITH "J"
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 9/15/10, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:7018] SDSS consumable procurement
To: materials-welding@googlegroups.com
Date: Wednesday, September 15, 2010, 2:22 PM

Dear All,
 
I have to fill an order form for welding consumable procurement for SDSS material ASTM A928.
Consumable selected SFA/AWS 5.4   E2594-15
Process - SMAW
 
The consumable manufacturer need some information from our side.I am able to provide a few.I have no idea about the question mark I provided.It will be highly helpful,If any one have any idea or can give some guidance to fill this form 
 
Welding
 
1.PWHT - ?
 
2.Radiography/soundness test - ?
 
3.Fillet weld test - ?
 
4.Bend test - ?
 
5.Other .......... ?
 
Chemical Analysis
 
1.Ferrite content - Found from client spec
 
2.Moisture content - ?
 
3.Diffusible hydrogen - ?
 
Mechanical Testing
 
1.Yield strength - Found from ASTM
 
2.Tensile strength - Found from ASTM
 
3.Impact test - Found from client spec the required impact energy
 
4. Lateral expansion - ?
 
4. Hardness - Found from client spec 
 
 
What is Test schedule according to 5.01, ie Schedule F, G,H,I,J and Schedule K?
 
 
 
From where I can get these data.Rest of the data I found from client specification.
 
Please share ,If any one have previously used format for the same 
 
 
Regards,
 
Limesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...