Dear All,
I have to fill an order form for welding consumable procurement for SDSS material ASTM A928.
Consumable selected SFA/AWS 5.4 E2594-15
Process - SMAW
The consumable manufacturer need some information from our side.I am able to provide a few.I have no idea about the question mark I provided.It will be highly helpful,If any one have any idea or can give some guidance to fill this form
Welding
1.PWHT - ?
2.Radiography/soundness test - ?
3.Fillet weld test - ?
4.Bend test - ?
5.Other .......... ?
Chemical Analysis
1.Ferrite content - Found from client spec
2.Moisture content - ?
3.Diffusible hydrogen - ?
Mechanical Testing
1.Yield strength - Found from ASTM
2.Tensile strength - Found from ASTM
3.Impact test - Found from client spec the required impact energy
4. Lateral expansion - ?
4. Hardness - Found from client spec
What is Test schedule according to 5.01, ie Schedule F, G,H,I,J and Schedule K?
From where I can get these data.Rest of the data I found from client specification.
Please share ,If any one have previously used format for the same
Regards,
Limesh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment