Hi,
Please find herewith the attached file of electrode selection table.It might be useful to you.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 9/13/10, r.kesav moorthi <k7moorthi@yahoo.co.in> wrote:

From: r.kesav moorthi <k7moorthi@yahoo.co.in>
Subject: Re: [MW:6971] Re: What is the consumables for following welding material
To: materials-welding@googlegroups.com
Cc: vanchinaths@gmail.com
Date: Monday, September 13, 2010, 12:09 PM

Hello Mr. Vanchi
1.) 11Cr Cb+11Cr Cb- 3.0mm thick/650-750 deg celcious, any of the following Process SMAW,FCAW,TIG,GMAW & Butt & FIllet both Qualification ( Pre heat, PWHT & Consumable ).
2.) SA 387 Gr.11 ( 6mm) + AISI 304( Rod dia.60) / 650-750 deg celcious
fillet weld Qualification -SMAW( Pre heat, PWHT & Consumable).
 bot shall be As per ASME SEC. IX
 
Thanks & Regards

 
175, R.Kesavamoorthi,
Principal surveyor,
Quest (pvt.) Ltd.,
Ranipet.



From: vanchi <vanchinaths@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Sat, 11 September, 2010 11:43:23 AM
Subject: [MW:6952] Re: What is the consumables for following welding material

pl specify thk and design  temperature to decide about the selection
of consumable. Incase PWHT is involved selection will change. what is
the code of construction?

On Sep 9, 12:39 pm, "r.kesav moorthi" <k7moor...@yahoo.co.in> wrote:
> Sir,
>
> I want to know the consumable for welding following materials
> 1.) 11Cr Cb+11Cr Cb- SMAW,FCAW,TIG,GMAW( Pre heat, PWHT & Consumable ).
> 2.) SA 387 Gr.11 + AISI 304-SMAW( Pre heat, PWHT & Consumable).
>
>  
> 175, R.Kesavamoorthi,
> Principal surveyor,
> Quest (pvt.) Ltd.,
> Ranipet.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.