Dear Vinod,
It could be a self reinforced butt welded  nozzle to shell or a weldolet welded to shell and pipe attached to weldolet with butt joint.
vanchi
On Mon, Sep 13, 2010 at 9:07 AM, Vinod Jotwani <poojvin@yahoo.com> wrote:
Dear All,

We are taking up the jobs of replacement of one of the nozzle on our AFC . In the specs it is mentioned forged saddle type.

What does it mean by saddle type ?is it set in type or set on type.

Vinod




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...