Sorry its IS1030 340-570W and i Want its Equivelant ASTM?
All you said is known I want to check the ASTM equivelant for checking the Heat treatment temperatures for Normalizing and Tempering.
Regards
Sreedhar
On Sun, May 16, 2010 at 4:56 PM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
There could be typo error. It should have been either 280-520W or 340-570W. The former indicates YS and the later indicates UTS. Suffix W indicates weldable. These are carbon steel castings.
On Sun, May 16, 2010 at 3:52 PM, sreedhar ch <sdchitturi@gmail.com> wrote:
Dear friends,Can anyone in this group tell me the ASTM Equivalent grade for BIS 1030 Gr 340-520W.RegardsSreedhar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment