Tuesday, May 11, 2010

RE: [MW:5134] Galvanizing oh Handrail

Get "Design of Products to be Hot Dip Galvanized after Fabrication" from
www.galvanizeit.org.

Free download the American Galvanizers Association.

Bob Shaw
SSTC

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
welding_engr_rich@charter.net
Sent: Monday, May 10, 2010 8:40 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:5131] Galvanizing oh Handrail

During the cleanning process liquid such as sulfric acid and a neutizing
solution may not be drained from the handrail prior to imersion in the
galvaizieng dip tank. Without holes to vent the trapped gasses (Air, acid
or neutalizing solutions) the handrail will act like a bomb, causing an
explosive burst of molten zinc to be sprayed out of the dip tank.

Having been at a shop where this occured it is very scary and can cause a
significant amount of property damage and personnel injuries.

Best regards

Richard M. Beldyk PhD, PE
AWS Certified Welding Engineer
ASQ Certuified Sx sigma Black Belt


Original Message:
-----------------
From: Vijay k.vijayaraj@gmail.com
Date: Sun, 9 May 2010 11:46:28 -0700 (PDT)
To: materials-welding@googlegroups.com
Subject: [MW:5121] Galvanizing oh Handrail


Dear All,

We are fabricating handrails for our client. That to be galvanized
externally. I heard that proper holes to be provided on the handrail
for vent to dip the handrail while doing dipping. Is it is necessary?

Kindly guide me on this.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.


--------------------------------------------------------------------
myhosting.com - Premium MicrosoftR WindowsR and Linux web and application
hosting - http://link.myhosting.com/myhosting


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...