Re: [MW:5122] Galvanizing oh Handrail

Yes, the vent holes are drilled in order to provide an escape routefor the hot gases and molten zinc failing which the handrails will come out bent from the galvanizing bath/Cooling bath.
 
Mohammad Afzal Baig
On Sun, May 9, 2010 at 9:46 PM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear All,

We are fabricating handrails for our client. That to be galvanized
externally. I heard that proper holes to be provided on the handrail
for vent to dip the handrail while doing dipping. Is it is necessary?

Kindly guide me on this.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Mohammad Afzal Baig
````````````````````````````````````````` email:afzal1972@gmail.com
       


 
     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...