Monday, May 10, 2010

[MW:5123] RE: 5121] Galvanizing oh Handrail

Hi Vijay,
It is mandatory to avoid any incidents during the hot dip galvanizing
process.
Your vendor should be able to provide the detail guidelines on those
vent holes of at least 10mm in diameter at both end of the handrailings

Thank you,

Best Regards.

David Chan
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Vijay
Sent: Monday, May 10, 2010 2:46 AM
To: Materials & Welding
Subject: [MW:5121] Galvanizing oh Handrail

Dear All,

We are fabricating handrails for our client. That to be galvanized
externally. I heard that proper holes to be provided on the handrail
for vent to dip the handrail while doing dipping. Is it is necessary?

Kindly guide me on this.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step