qualificated the WPS used? as a butt weld? as a buttering weld?
On May 18, 6:46 pm, Dindo <dindodelac...@gmail.com> wrote:
> You can do this by making sure that the weld to be welded on is clean and
> smooth to prevent any inclusions, you can use your orginal WPS.
>
> On Tue, May 18, 2010 at 8:36 AM, fer <fernando.alvarez.f...@gmail.com>wrote:
>
>
>
>
>
> > ASME VIII div 2 allows you to weld an attachment directly on the weld
> > overlay of a pressure vessel.
>
> > How should be qualified the WPS to carry out this welding?
>
> > The coupon of the PQR should be done with a buttering between the
> > material of the shell and the material of the attachment?
>
> > Could be asigned a P number to the weld overlay material and weld the
> > coupon between the P number of the overlay material and the P number
> > of the attachment?
>
> > Any idea would be helpful
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding-unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.