[MW:5033] RE: 5026] Pre Qualified Fillet Weld WPS as per AWS D1.1

Just stay within the limits of prequalification in AWS D1.1 Clause 3, and write a WPS for your 1F and 2F welds accordingly.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shahul
Sent: Monday, May 03, 2010 8:57 AM
To: materials-welding@googlegroups.com
Subject: [MW:5026] Pre Qualified Fillet Weld WPS as per AWS D1.1

 

 

 

Dear All,

We have qualified a single V groove welding procedure in 3G position as per AWS D1.1. With this procedure, i can only do 3G in groove and 3F in Fillet. So i have prepared pre qualified single V groove WPS for groove welding in all positions.

But we have some jobs which demand 1F and 2F positions. So, i want to know whether prequalified WPS for the single V which i made is acceptable for doing fillet welding in all positions?? Or is there any prequalified WPS for fillet available ??

--
Thanks and Regards

Shahul

QC WELDING ENGINEER
CSWIP 3.1, AWS CWI
Aasia Steel Factory Co. Ltd
KSA

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...