RE: [MW:4973] API 5L X85 -CVN Requirements

I heard that 44th edition of API 5L has 3 new grades X90, X100 and X120.
what is X85? CVN is mandatory for all PSL2 pipes, refer para 6.2.5.2


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Tuesday, April 27, 2010 3:53 PM
To: materials-welding@googlegroups.com
Subject: [MW:4966] API 5L X85 -CVN Requirements

Gents,
 
Pls tell me, what is the CVN (Longitudinal) Requirements for the API 5L X85 (19 mm thick) ?
 
Thanks & Regards,
 
K.Babu