Wrong! See ug-10 or Pg-10 depending on code section


  From: "Bathula Raghuram (Mumbai - PIPING)" [R.Bathula@ticb.com]
  Sent: 22/04/2010 02:37 MST
  To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
  Subject: RE: [MW:4920] Re-Certifying Material


You can prepare a comparison table of all chemical and mechanical properties for both grades and get it certified by AI (one such table is attached for ref)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramesh Barot
Sent: Thursday, April 22, 2010 2:34 PM
To: Materials Welding
Subject: [MW:4919] Re-Certifying Material

Dear All,
 
Pl.give me detailed procedure for re certifying material?
 
Example 1)ASTM to ASME
              2)AISI to ASME/ASTM
              3)ASME to ASME (Different edition)
 
Thanks,
With Best Regards,
Ramesh Barot