Monday, February 9, 2009

[MW:1513] RE: 1511] cheron crack detected by ut

TOFD will be the best option to find out such cracks…

 

Regards.

 

C. K. Purohit

General Manager - QC

KNM Process Systems Sdn Bhd - Malaysia

 

HP No. : 6016-3376448


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Sunday, February 08, 2009 3:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:1511] cheron crack detected by ut

 

hi

what is the suitable technique for detection chevron crack by ut or other ndt methods in thk>40?

thanks adv


 

 







***DISCLAIMER NOTICE ***

"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...