Hi all, TOFD is useful to size the crack once its presence is detected by regular UT techniques. Regards, Shashank Vagal
--- On Mon, 9/2/09, Chaitanya Purohit <ck@knm-group.com> wrote:
From: Chaitanya Purohit <ck@knm-group.com> Subject: [MW:1513] RE: 1511] cheron crack detected by ut To: materials-welding@googlegroups.com Date: Monday, 9 February, 2009, 11:01 AM
TOFD will be the best option to find out such cracks… C. K. Purohit General Manager - QC KNM Process Systems Sdn Bhd - Malaysia HP No. : 6016-3376448 From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of Ali Asghari Sent: Sunday, February 08, 2009 3:24 PM To: materials-welding@googlegroups.com Subject: [MW:1511] cheron crack detected by ut what is the suitable technique for detection chevron crack by ut or other ndt methods in thk>40?
***DISCLAIMER NOTICE ***
"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."
Add more friends to your messenger and enjoy! Invite them now. --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-