Skip to main content

Re: [MW:31603] WPS and PQR According to ASME Sec.IX and Sec.VIII- Boiler and Pressure Vessel Code

Dear Sir,

For welding qualification ( WPS )
You have to follow ASME- IX , not ASME VIII

Thanks & Regards,

On Sat, Oct 24, 2020 at 6:59 AM K K <karan.hbl@gmail.com> wrote:
Dear Experts,

Please refer below WPS and PQR details.

PQR Details - Base Metal - ASTM A106 Gr.B  To ASTM A106 Gr.B. ( P No - 1 Gr.No - 1 To  P No - 1 Gr.No - 1 ).
Process - GTAW  + SMAW ( GTAW - 4.8 mm + SMAW - 13.46 mm)
Thickness of the Coupon -18.26 mm, Dia - 6"
With PWHT - 638°C ,time 72 min.
No Impact tested.
DESIGN TEMP. / MDMT (°C) -290 / 5 .

WPS Details - Base Metal - ASTM A106 / A516 Gr.B / Gr.70  To  ASTM A106 / A516 Gr.B / Gr.70 . ( P No - 1 Gr.No - 1/2 To  P No - 1 Gr.No - 1/2 ).
Process - GTAW  + SMAW ( GTAW - 9.6 mm + SMAW - 15.4 mm).
SFA No- GTAW - 5.18 and for SMAW - 5.1.
AWS No - GTAW - ER70S-3 and SMAW - E7018-1H4R.
Pre heat - less than 12.7 mm -10°C and less than 25 mm 75°C.
Inter pass Temp. -315°C.
PWHT - 620°C, Holding time 1 hr thk +1 hour min.

According to above details help me to review, as per ASME Section VIII for Boiler and Pressure Vessel Code.
And I need your suggestion what are the essentials requirements according ASME  Sec.VIII. And what are the important things i have to check.
Please suggested me with clause reference.

Please send me your valuable suggestions, it's Supports me lot.

Thanks and Regards
Kiran




 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c3e78183-f533-400b-bfe1-ba8e24f94c6an%40googlegroups.com.
--


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022




This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmSsDQqPOy0XJ__uyHX3_zaKxz5bo0QnO4drHd_ybGYzKw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...