Skip to main content

Re: [MW:31560] BIS Approved SS-316 Square Bar and Flat

As far as I think BIS IS NOT APPLICABLE FOR HSN 7222.

Both items fall under 7222.

Kindly check for the same.

On Tue, 13 Oct 2020, 19:52 Vinod Kataria, <vinod.kataria@blissanand.com> wrote:

Dear All,

For one of our Saudi Aramco Project we need to source following material:-

 

ITEM

QTY

UNIT

SQUARE BAR 40MM (TOL +0.0/-0.4MM) SS-316/316L (Finish length 431 mm-01 no's, 1089 mm-02 no's.)

50

KGS

RECTANGULAR STRIP SIZE 76 X 25MM, SS-316/316L (Finish length 360 mm-06 no's , 210 mm-04 no's)

50

KGS

 

MTC as per EN 10204 3.1 minimum.

Material shall be annealed condition as applicable.

NACE MR-01-75 / ISO 15156 shall be complied.

Material shall be procured from Saudi Aramco approved vendor.

 

We have placed our order on UK supplier and now when material is ready we understand from our commercial department that BIS (Bureau of Indian Standard) approval is a must to import any material so we requested the supplier and got following response:-

 

"To obtain BIS approval is not that easy, it involves a complete audit in order to firstly obtain the BIS registration,

and then once we have obtained the approval we have to submit documents for each export order for approval.

 

This would take some weeks and would be costly."

 

Can anyone from their past experience suggest me how to come out of this situation….thanks in advance for your time and help.

 

Regards,

Vinod Kataria

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/TY2PR0101MB29426CB7ED5A9FC75FE74EC287040%40TY2PR0101MB2942.apcprd01.prod.exchangelabs.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPU1SNuSDvc4Q%3Dxza8eAAW6gZHRGHEUmXvySjQEDWTrOggkvow%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...