Skip to main content

Re: [MW:31576] WPS from AWS to BS Standards

Welding position here is as per ISO 15614-1 Not AWS D1.1 as i said before and clearly mentioned in WPS and subject title 
as per ISO 15164-1 

This means only PG and H-LO45 need to be separately qualified , and if qualified for any position all other position will be qualified except PG and HI-LO45 
My case here in over head welding (5G See below Sketch ) so PG will cover all position expect HI-LO45 


For Current and voltage this values are taken already from actual WPS/PQR but according to AWS D1.1 as i told you i need only to convert it to BS EN 
this Preliminary WPS as you know actual values will be recorded and written during running of final PQR 
Trade name and brand is not mandatory variable here too 

Hope it is clear now 

Regards,
H.A


On Tue, Oct 20, 2020 at 7:19 PM Mayur Hiremath <hiremath.qaqc@gmail.com> wrote:
Hello, 

PG will not cover 6G, Refer attached Welding positions.

Also need to change the Current , voltage according to Consumable Manufacturer Data sheet as per the thickness of electrodes. Then heat input <=3KJ/mm.
When preparing pWPS parameters need to consider as per data sheet of consumable.
Regards,

On Tue, Oct 20, 2020, 6:43 PM Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear  Vinoth / Experts 

i had prepared preliminary WPS as per  ISO 15614-1  so please check all parameters and inputs are ok or not 

additionally , check if this cover welding positions up to 6G and steel grade S355 and thickness up to 32mm 

Appreciate your fast action and assistance 

Regards,
H.A

On Sat, Oct 17, 2020 at 7:40 AM Hani Al Masry <hanyonalfy@gmail.com> wrote:
 
how about 

·                  BS EN ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys


what is the major changes i need to made to the current WPS to convert it from AWS to 



On Fri, Oct 16, 2020 at 7:29 AM Vinoth Rajendran <rajvinoth1987@gmail.com> wrote:
Please go through EN  ISO 15609, EN ISO 15614-1, EN ISO 9606

On Thu, Oct 15, 2020, 18:47 Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear Experts 

Our client is asking to convert our WPS from AWS to BS Standards
can you please advise 
which BS standards we need to use 
what the mean steps to be changed according to this BS 
Requirement of back stip for pipe welding 

Regards,
H.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfjuGE1OGLGRz%2B7gY0syR5F8ifC9jRFWdyzzR3n7bZDXA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba0BHbLE%2BRtObsF4XaaMcen325c4QbBTeGs4DK5VDC%2ByeQV%2Bg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzeQ36kA5njY74o4nv-c8QPGy7mmKGc4XywouR3mbmCFEg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGQ515wG_%3DMQkEYDQDTVYdM8pW161EpHdbJ_p2MZzqUcDY8jBA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzf_kjM4EoG-WJiB%3DGJQP26NH_-bwBDkhQ5M3_%3DT3SjmPQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...