Hello,
In the syllabus for AWS CWEng exam, two surfacing process are mentioned as SW, THSP. Anyone have idea what it is?
Reference AWS B5. 16
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3bcd2ac8-808f-408b-ad0b-18cc360819be%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs
Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...