Re: [MW:30846] PWHT Requirements and Material Selection

The material 516 Gr 70 is a P1, you are mentioning that it is a repair, I suggest you check Table UCS-56-1 (b) (ASME Section VIII Div. 1), where the PWHT requirements for P1 materials appear, in ( b) it makes some exceptions to the PWHT based on the thickness of the material, if you exceed those thicknesses you will have to do the PWHT, but because it is a repair you also have to check the NB-23 and API 650 since from what I see in the drawing is a kit for the O&G Industry.
The Skirt I do not think it should carry PWHT since it is not a pressurized part.
Cheers!.

El mar., 5 may. 2020 a las 1:31, 'TC Kwa' via Materials & Welding (<materials-welding@googlegroups.com>) escribió:
Hi,

If it is for Sour service, PWHT shall be done, since material is A-516 Gr 70.
Thank you. 


Regards,

Ir. TC Kwa

+6012-3998739

Email: tckwa@yahoo.co.uk

LinkedIn Profile : https://my.linkedin.com/in/tckwa 





On Tuesday, 5 May 2020, 12:36:46 GMT+8, enginakgun55 <enginakgun55@gmail.com> wrote:


Hello,

We work on material selection about column materials (shell, head, skirt). If we use A-516 Gr.70 material in this project, does it require heat treatment for repair on the column during maintenance?


Production Properties : Sour Service , Distilation Column

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8e5362b-3f5e-4fdc-912f-cc390d512800%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/601900513.2557215.1588657191572%40mail.yahoo.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJzZKoh7ksS5u6LqF5ozWO2rKeVaW0rOOMLTtepqCWsaA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...