Dear Members,
I'm m here to clear my dout regarding welder qualification diameter range.
With respect to asme sec 9 QW 452.3, a welder test coupon in the range of 1 inch(25) to 2 7/8(73)..he qualified 1 inch(25) and above..[for ref: plz go through ASME SEC-9].
My dout is :-
(1) In bracket ( as per QW-452.3 ) mentioned reading belongs to NPS or OD....???
(2)Does he is qualified to do welding on 3/4 inch. Pipe With above mentioned range...??
Please help me...
Regads,
Shersha shereef
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment