Sureshkumar Pethureddy: I think your explanation about the possible origins of these two concepts (Hp / LP) is quite good, I agree with you and how well you clarify them are not concepts that are standard or that are defined in any standard or code, as you say they are part of the ARGOT, or they fit in my country of the "farandula"; In the end, each client can make their own requirements very specific to their project, just take into account that there are no written guidelines to which we can refer to give form or strength to these customer requirements, the only requirement is the client and in this case it is the client that has to define it, clearly explain what it needs.
Regards!.
El dom., 10 mar. 2019 a las 0:08, steel_microbe (<matschka69@gmail.com>) escribió:
--There is nothing in the codes pertaining to this Hp / LP. Years ago, welders who welded heavy wall Cr. piping that was pre heated in fossil fuel plants were calledHOT WELDERS. This was a slang term that probably started in a bar after work. The term has persisted somewhat as these welders still refer to themselves as 'HOT WELDERS.' The term (H)igh (P)ressure welders originated in the same way. This term again refers to a welder who welds on the high temperature, high pressure Main Steam lines which are pre heated. These welders were considered the BEST welders because they had to perform these welds while enduring the high temperatures from the pre-heating equipment. Consequently they worked thru dinner time & got overtime as a bonus. These welds are heavy wall like 2-3 inchs or more and are X-Rayed & stressed relieved. A High Pressure, HP. welder is an archaic term. Nevertheless these guys are considered the 'crème of the crop. LP has to mean a Low Pressure welder. One who welds on water lines, no X-Ray, etc. If your client wants you to categorize your welders HP & LP I don't see a problem. You should now which welders that are qualifying are really good, and which welders are just so-so. And your inspectors in the field should knowwhich ones are really good and those who are average.
On Friday, March 8, 2019 at 3:11:14 AM UTC-6, sureshkumar wrote:DearPlease check project specification/vendor procedure/Li censor procedure, nothing given make one letter to client to clarify
regards
suresh
On Fri, Mar 8, 2019 at 11:10 AM José Juan Jiménez Alejandro <jjjim...@gmail.com> wrote:Frankly I had never heard these two concepts, at least they DO NOT EXIST IN ASME, and it did not seem logical to me that they will be linked to a specific type of material. regards!.--El jue., 7 de marzo de 2019 9:47 p. m., Hareesh K V <haree...@gmail.com> escribió:Dear All,--At least one person (Mr. José Juan Jiménez Alejandro) asked that question "which is the code?"
To avoid serious before commenting please ask the background.Which is the construction code?ASME B31.1, ASME B31.3 or any other (IBR 1950- India Boiler Regulations )"May be because of quality issues. Client afraid, interchange the filler wire for HP (P91) LP( P22 or P11)"In which code it is written that HP is P91 and LP is P22/P11?HP, LP etc are design basis and cannot be linked to a particular material.Regards,Hareesh K V+91-8547859202On Fri, Mar 8, 2019, 6:18 AM José Juan Jiménez Alejandro <jjjim...@gmail.com> wrote:CODE???--El jue., 7 de marzo de 2019 10:30 a. m., Arun Kumar.P <arun...@gmail.com> escribió:Hi,--May be because of quality issues. Client afraid, interchange the filler wire for HP (P91) LP( P22 or P11)Regards,Arun
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Ing. José Juan Jiménez Alejandro
ASME Independent Consultant
and Technical Manager SSI-TPI
Cel. +52 812 352 4606
Skype: jjjimeneza
Twitter: @jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment