Tuesday, July 3, 2018

Re: [MW:28027] ASME SEC-2 PART A CLARIFICATION

Hi,

Code gives max limits, there is no min limit. So the material grade will be GR 70 only.

On Tue, Jul 3, 2018 at 8:36 AM, SARAVANAN KRISHNAN <saravweldingengineer@gmail.com> wrote:
Dear Experts.

As per ASME CODE SECTION 2 PART A  SA 516 Gr 70 material chemical composition,carbon minimum value does not shown.
Due to our project,   SA 516 Gr 70 material chemical composition of carbon value is 0.18.so i will consider as a Grade 55?

please explain the above query. Thanks in advance.

--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     SR QA/QC ENGINEER,
      DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Dsilva

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...