Re: [MW:28025] ASME SEC-2 PART A CLARIFICATION // SA 516 Gr 70 material Low carbon values

No, C values specified are maximum in code . you need to meet strength too. stick to the grade what is specified by your designer

On Tue, 3 Jul 2018 at 09:16, SARAVANAN KRISHNAN <saravweldingengineer@gmail.com> wrote:
Dear Experts.

As per ASME CODE SECTION 2 PART A  SA 516 Gr 70 material chemical composition,carbon minimum value does not shown.
Due to our project,   SA 516 Gr 70 material chemical composition of carbon value is 0.18.so i will consider as a Grade 55?

please explain the above query. Thanks in advance.

--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     SR QA/QC ENGINEER,
      DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...