The main difference is that EN 10204 is harmonized to the European Pressure Equipment Directive, and material certificates for materials for pressure equipment to be CE marked to that directive need to be in accordance with EN 10204.
EN 10204 refers to another EN-standard giving instructions on what should be stated in the certificates.
Kind regards
Kristian
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohan
Sent: 2. juli 2018 14:35
To: materials-welding@googlegroups.com
Subject: [MW:28017] ISO 10474 Vs EN 10204
Dear Experts,
Can any body please tell me if there is any difference between ISO 10474 Vs EN 10204
Regards
G.Mohanraj
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments